Beilstein J. Nanotechnol. 2018, 9, 2628–2643, doi:10.3762/bjnano.9.244
Figure 1: SEM images, a) top and b) cross section, of TNTs for each of the anodization times (ta): c) 0.5 h, ...
Figure 2: High-resolution XPS spectra for Ti 2p, O 1s, F 1s and N 1s obtained for the TNTs after each ta.
Figure 3: X-ray diffraction patterns of TNT grown at different ta.
Figure 4: Raman spectra for TNT grown at different ta. Laser intensity: 2.5 mW/cm2.
Figure 5: (a) Cyclic voltammograms (CV) at v = 50 mV/s; and (b) linear-sweep voltammograms (LSV) at v = 5 mV/...
Figure 6: Extracted photo-current density, jph, from potentiodynamic curves for the TNTs grown at different ta...
Figure 7: (a) Incident photon-to-current (IPCE) plot for each TNT. (b) Tauc plots for a direct electronic tra...
Figure 8: a) Mott–Schottky plots recorded at f = 400 Hz in 0.5 M H2SO4. The electrode potential range was fro...
Figure 9: a) Schematics of the experimental setup used for the PEC degradation of MB. b) UV–vis spectra for t...